back to top
My wish lists
Save your wish list
If you want to add more content to your wish list, simply log in. If you do not have a user account, please register for the Hanser Customer Center.

» Do you already have a user account? Please log in here.
» Don't have a user account yet? Please register here.
Your wish lists
If you want to use your wish list during your next visit, simply log in. If you do not have a user account, please register for the Hanser Customer Center.
» Do you already have a user account? Please log in here.
» Don't have a user account yet? Please register here.

« Back

Your advantages at a glance

  • One login for all Hanser portals
  • Individual home page for faster access to preferred content
  • Exclusive access to selected content
  • Personal wish lists on all portals
  • Central management of your personal information and newsletter subscriptions

Register now
Deutsch
Bookmark Bookmarked
Journal of Plastics Technology 2006/01

Anwendung der Maskentechnik beim Laserschweißen mikrostrukturierter Kunststoffbauteile

Particularly, the mask technology, a process variant of laser transmission welding, is suitable for the application in micro technology. In fundamental investigations at the IKV Aachen it has been examined, which structural dimensions can be realized using the mask technology and how the different welding parameters influence the welding process. Moreover, the suitability of this process for the welding of a complex microfluidic structure has been shown.

Prof. Dr.-Ing. E. Haberstroh | Dipl.-Ing. W.-M. Hoffmann | Dipl.-Ing. R. Lützeler
Institut für Kunststoffverarbeitung (IKV)

These articles might be interesting for you
Further Information

The Journal

The Journal of Plastics Technology is a peer reviewed internet periodical published under the auspices of the Scientific Alliance of Polymer Technology (WAK)


Further Information and Contact


Editorial Board


WAK-Homepage

International Polymer Processing

International Polymer Processing, the journal of the Polymer Processing Society, is a discussion forum for the world-wide community of engineers and scientists in the field of polymer processing.

The journal covers research and industrial application in the very specific areas of designing polymer products, processes, processing machinery and equipment.


International Polymer Processing


Top 20 Article-Downloads

Scopus indexed
Scopus

The Journal of Plastics Technology is indexed in SCOPUS, the largest abstract and citation database of peer-reviewed literature.